1

Topic: repetier host and solidoodle 4 not working

Hi have had a problem here last couple of days Repetier connects to machine, heats bed and extruder but wont print .   It starts moves to center of bed then stop.  Repetier then locks up.   Any suggestions. thanks in advance

2

Re: repetier host and solidoodle 4 not working

It sounds like it is waiting for a temperature to reach its start point.

SD2 Expert stock, ABS fume fan,
XYZ DaVinci 1.0 stock ABS, Simplify3D
QUBD Two-Up PLA, new 3D printed X gantry, Y idler, flex z coupler, extruder mount, E3D Lite

3

Re: repetier host and solidoodle 4 not working

I believe I found what problem is.  I imported a g-code from kisslicer and it starts but stops at center of bed.  Then program crashes have to reinstall printer drivers then works.  But what would make the program crash?  Ggunners thanks for the reply

4

Re: repetier host and solidoodle 4 not working

Did you find out what was the cause?  My SD4 two weeks old suddenly doing the same thing.
Thanks,
J.P.
SD4- ABS

JP
Solidoodle 4 STOCK
purchased 5 AUG 2014