Topic: Shaft collar rubbing on flange
Hi folks,
I have a filastruder v1.5. I have followed the instructions up until step 6. At this point, I observed that the bearings are on the opposite side of the flange, and thus the shaft collar rubs directly against the flange. Realizing this can't be right, I turn to you for help.