1

Topic: Acrylic Extruder upgrade to Aluminum

Would there be any interest in a replacement extruder made from aluminum that would replace the acrylic?  I noticed a crack in mine and decided to replace with aluminum.  It would not include the hardware as you would unbolt/rebolt your existing hardware.  Target price would be around $30, but should be the last one you need to replace.

2

Re: Acrylic Extruder upgrade to Aluminum

WHAT MODEL DO YOU HAVE?
I saw that Solidoodle has shipped the SD 4 with a all-new extruder now,
If you check their website, in Spare Parts they have the alum. Extruder.

3 (edited by ohbaby714 2014-05-23 13:59:43)

Re: Acrylic Extruder upgrade to Aluminum

I'm interested, did you have some made already?
If so, picture please.

Oh yea, BTW, I have an SD3.

4 (edited by MacGyverX 2014-05-27 13:59:31)

Re: Acrylic Extruder upgrade to Aluminum

It is possible to use the SD4 extruder parts on the SD2. Two mods needed to be done for this to work. The bridge piece needs to be extended 2.2mm and a plate needs to be made to mate with the two long bolts under the extruder to the two holes in the stepper.

The plate in the image below was temporary. I've since created and cut out a nicer looking one.

Post's attachments

ZZ441984CB.jpg 662.31 kb, file has never been downloaded. 

ZZ5A95FE9E.jpg
ZZ5A95FE9E.jpg 1.01 mb, 1 downloads since 2014-05-27 

ZZ7F49E8B8.jpg 885.37 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.
SD Press - v1 (Pre-order) / RAMPs /w DRV8825's / Cyclops (25w) / Dual Bowden / Mk8 Gear / MK2b PCB Heat bed /w custom replacement Z / PEI Bed
SD2 / E3D v6 / Direct Drive / Mk8 Gear / RAMBo v1.3 / PEI Bed / Anti Z backlash mod / Ikea Expedite enclosure.
Both Driven by Octoprint (devel) via a RPi B+ / Neopixel status alerts / GPIO Controlled SSR / (SD2) 450 Watt PSU for remote power-up/shutdown.

5

Re: Acrylic Extruder upgrade to Aluminum

I think Mac did a very nice job, see it,
just make a 2mm thick alum. Plate with 4 holes,
Or print one as an adapter, then you can
Mount a SD4 new metal extruder to SD 2 & SD 3
S X-carriage, like Mac's second picture to show.

6

Re: Acrylic Extruder upgrade to Aluminum

Mac,

Is that the same tension spring from the old acrylic extruder?
What parts did you actually get?
I'm guessing that i can use the same hardware that i already have from acrylic one.

Block:
http://store.solidoodle.com/index.php?r … uct_id=149

Arm:
http://store.solidoodle.com/index.php?r … uct_id=152

PEEK:
http://store.solidoodle.com/index.php?r … uct_id=145

7 (edited by MacGyverX 2014-05-28 12:35:02)

Re: Acrylic Extruder upgrade to Aluminum

It did not include the spring. That I got from a assorted pack from Home Depot (4.99 for 50 assorted springs).
The new parts came with screws. The only part from the old jigsaw I use was the long screw that held the tensioner to act as a guide for the spring.

SD Press - v1 (Pre-order) / RAMPs /w DRV8825's / Cyclops (25w) / Dual Bowden / Mk8 Gear / MK2b PCB Heat bed /w custom replacement Z / PEI Bed
SD2 / E3D v6 / Direct Drive / Mk8 Gear / RAMBo v1.3 / PEI Bed / Anti Z backlash mod / Ikea Expedite enclosure.
Both Driven by Octoprint (devel) via a RPi B+ / Neopixel status alerts / GPIO Controlled SSR / (SD2) 450 Watt PSU for remote power-up/shutdown.

8

Re: Acrylic Extruder upgrade to Aluminum

Awesome, thank you.

How is it perform compare to the old acrylic one.
I'm guessing reloading should to be an improvement with the spring loaded.
Also the spring eventually need to be replace after a while?

9

Re: Acrylic Extruder upgrade to Aluminum

It's performed perfectly. I've done 7 prints since the mod. All avg. 2 hours. My favorite part of the mod is the easy filament swap-out/installation. And no fear of cracking it. The 'upgrade' was fairly inexpensive. The only odd thing about the filament tensioner was it didn't come with the spring. (Even thou the description said 'Fully Assembled'.) Hopefully they won't jack the price up if people start doing this mod.

SD Press - v1 (Pre-order) / RAMPs /w DRV8825's / Cyclops (25w) / Dual Bowden / Mk8 Gear / MK2b PCB Heat bed /w custom replacement Z / PEI Bed
SD2 / E3D v6 / Direct Drive / Mk8 Gear / RAMBo v1.3 / PEI Bed / Anti Z backlash mod / Ikea Expedite enclosure.
Both Driven by Octoprint (devel) via a RPi B+ / Neopixel status alerts / GPIO Controlled SSR / (SD2) 450 Watt PSU for remote power-up/shutdown.

10

Re: Acrylic Extruder upgrade to Aluminum

That the problem i keeps having with the acrylic and plastic parts.
The acrylic cracked on me after less than a month and i went to jigsaw. It work great but eventually wear out on me.

Hopefully this mod will give me a more consistence clamp pressure with only one part that can wear down.
Periodic spring change probably all i need to worry about after the mod.