I have used the following so far:
-Regular kapton + ABS = issues with warping and sticking to the bed
-Regular kapton + hairspray + ABS = issues with warping and sticking to the bed but a lot better than without hairspray
-A4 copy paper + ABS= works suprisingly well but it leaves pieces of the paper on the printed parts
-Regular kapton with glass on top + ABS = issues with warping and sticking to the bed
-Regular kapton with glass on top & hairspray +ABS = issues with warping and sticking to the bed
-Regular kapton with glass on top & slurry (thin pieces abs and aceton mixture) +ABS =works very well so far, no warping at all
-Regular kapton with Plywood on top + ABS works well but needs more testing
-Regular kapton with fiberglass wallpaper on top + ABS .. testing at the moment.... seems to work
-A4 copy paper + Nylon (taulman 645) = works ok but not very good also (this might work with some more testing)
-Regular kapton with glass on top + Nylon (taulman 645) = issues with warping and sticking to the bed
-Delta terry-net + Nylon (taulman 645) NOTE: on a cold bed= works well (Delta terry-net is some medical aid undercast material I had laying around)
All tested with the bed at 95 celcius except for the last one. Are you guys having some good results with other printbed surfaces also?