Topic: Print Bed only heats up to 68°C
Hey!
I am having a problem with my print bed (SD 2). It only heats up to 68°C even though it should be at 95..
I can barely make my part stick to the bed. I never had that problem before and it has nothing to do with the room temperature. I always printed on 95°C and never put the case over my Solidoodle - I have no idea what's wrong.
Any ideas?
Thanks,
Salocin