I got my printer about a month ago and have been having very weird results.  I am new to the 3d printing community so i don't know a whole lot.  The problem is my prints sticking.  I have found using aqua net works most of the time but eventually the print keeps warping and ends up like this.  It also eventually comes off if it is a long enough print.  Please help! I want to start getting good prints.

Post's attachments

photo.JPG 1.18 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: warped bed? uneven?

I can't tell from the Picture if that is solid or not?  I assume not so first things first turn on about 5mm's of brim.
Second go buy a cheap 8"x8" piece of cheap glass at any hardware store.  Spray both sides of the glass it will stick to the Kapton tape pretty well after you cycle the heat a couple of times.  Adjust your Z-height to compensate for the glass and make sure the bed is perfectly level in relation to the nozzle.  Then using that same print with let the brim start to print and adjust the Z-height until the ABS is squished nicely to the bed.  I don't know what temp you have the bed at but I find more heat is a good thing.  I use 108 but 100 to 105 should work.
Hope this helps and Happy Printing.

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions

3

Re: warped bed? uneven?

wardjr is dead on. My bed warped about a month after receiving it. You can check warpage by laying a straight edge on it. If it is brand spanking new, contact Solidoodle and they may send you a new one if you send them an image of the warpage with a straight edge.
OR! If you do not trust UPS and are impatient, do like he said. I bought 2 mirrors at a local glass store for like $8. Superior to printing on Kapton (in my experience), and it looks neat. If you by a 1/8" thick cut of glass, it won't warp to the curvature of even the warpiest warped bed. If it does, it would take a very long time.

Printit Mason and Printit Horizon printers
Multiple SD2s- Bulldog XL, E3D v5/v6/Lite6, Volcano, Hobb Goblin, Titan, .9 motor, Lawsy carriages, direct Y drive, fishing line...the list goes on
Filawinder and Filastruder #1870.....worth every penny!

4

Re: warped bed? uneven?

AZERATE wrote:

wardjr is dead on. My bed warped about a month after receiving it. You can check warpage by laying a straight edge on it. If it is brand spanking new, contact Solidoodle and they may send you a new one if you send them an image of the warpage with a straight edge.
OR! If you do not trust UPS and are impatient, do like he said. I bought 2 mirrors at a local glass store for like $8. Superior to printing on Kapton (in my experience), and it looks neat. If you by a 1/8" thick cut of glass, it won't warp to the curvature of even the warpiest warped bed. If it does, it would take a very long time.

well you see i bought some glass but when i put it on the glass wouldn't lay flat because i think the metal bed is warped, could this be?

5

Re: warped bed? uneven?

YES! it could be.  I had the exact same problem.  Get them to replace it, use a piece of glass.  Or do what will improve your machine.  I don't know about the Solidoodle 4, but 3 and below had stupid underpowered power supplies which really cause serious performance issues with your bed heater and hot end. 

Upgrade your power supply to something in the realm of a 12V 20 amp - 30 amp, or more.  You can pick up 12 V server power supply brand new off ebay for about $10.  Mine was a 54 amp 12 volt supply. You have to be handy with a soldering iron to do the conversion.  But well worth the time in my opinion.  Although maybe Solidoodle has since supplied better power supplies with the machines.  Anyhow the reason to upgrade is because your bed heater will work much better, and will allow you to upgrade your bed to a piece of granite or thick glass. I prefer granite. Here's a link to my bed upgrade with pics.