1 (edited by BFresh 2013-05-21 17:18:41)

Topic: Original Solidoodle configs + post your own

If like me you have modified the original solidoodle 0.1 and 0.3 config files to a point where you can't get them to work right anymore and could do with starting again using the originals, here they are...

I couldn't find them on the solidoodle website and had to download and instal repetier again to get them.

Also, if you've got some particularly good config files of your own, feel free to post them too with details of what they are for, and maybe photos of results too. (i.e. config for speedy printing, or config for super smooth printing). I know someone managed to get good results with 0.05mm layer heights.

Post's attachments

Solidoodle 0.1mm.ini 2.75 kb, 41 downloads since 2013-05-21 

Solidoodle 0.3mm.ini 2.76 kb, 35 downloads since 2013-05-21 

You don't have the permssions to download the attachments of this post.
Industrial Designer
Fresh Design Works (UK)
www.freshdesignworks.co.uk

2

Re: Original Solidoodle configs + post your own

This is a great Idea. I need the stock ones! I ran into the same problem. Thanks!

3

Re: Original Solidoodle configs + post your own

I have just finished testing a profile I have been working on. This is a good places to start if the solidoodle configs aren't working for you.

These settings seem to be the best working yet for solid parts and general printing. I've tried the profile on 2 different printers, one with glass bed and cover, and one without both, and the results were more or less the same.
The finish of the first layer is pretty good too, but I've done better by manually adjusting the flow-rate on the fly. I plan to improve this profile further.

Post's attachments

0.3 Solid 100613.ini 2.85 kb, 39 downloads since 2013-06-11 

You don't have the permssions to download the attachments of this post.
Industrial Designer
Fresh Design Works (UK)
www.freshdesignworks.co.uk

4

Re: Original Solidoodle configs + post your own

Anyone got a good 0.2mm profile?

Industrial Designer
Fresh Design Works (UK)
www.freshdesignworks.co.uk