Topic: Printing issues (Walls look like slinkies)
I'm trying to figure out what might be causing my prints to look so horrible.
I have printed several different types of squares and cubes and the sides are see through.
The layers are not sticking together.
When I first got my SD3 I leveled the bed, printed and everything was perfect.
Now I had to get a new Acrylic Assembly with a new hot end, plus I reloaded my laptop and had to reinstall all the software.
Steps I have taken:
Leveled bed
Calibrated the Extruder
Tested flow rate with a cube and it shows .41mm wall thickness
Upgraded from REP .85 to .95, they both do the same thing.
It seems that I'm just missing a setting but I'm not sure what.
I have read so much on the forums with different suggestions that I don't want to do anything counter productive.
Any ideas would be awesome.
***Forgot to mention***
Temps are 195 and 95
Bottom of cubes print perfect and are very strong.
Thanks in advance.