Topic: Set it and Forget it
Or not... Ive had my printer for a while now and I have my extrusion and flow rate locked down. The X and Y axis are pretty much right on the money. My Z axis on the other hand is really driving my nuts!
Say I print a cube thats 5mm tall and it prints 4.9 and i do the math print it again and its 5mm, sweet! So then i print a calibration vector next and its 30mm tall. Having JUST calibrated it it should be on point but no it prints out to be 31.49 or something. I do the math AGAIN print it out and its good. So now it should be good right ? I print the cube again and its 4.9 or something again!
Same thing happens with different layer heights. Ill have it printing 5mm cubes in ~.3mm but in ~.2 or ~ .1 it needs re calibrated.
Is this because of the 5/16ths lead screw? Ive even tried using the adjusted layer heights like .3034 , or .1058 still get this inconsistency in my Z axis.
Or is this just how it is at this point in these machines? There is no truly calibrated machine?