Topic: Warning - BAD ABS supplier

After having nothing but problems trying to print ABS with my SD2, I did a little research and discovered that KBELL Engineering (they sell ABS on Ebay) has had issues with their ABS, with a number of people having the same feeding problem that I have had.
http://feedback.ebay.com/ws/eBayISAPI.d … terval=365

I also was able to determine that the ABS filament they sell apparently comes from China.
http://www.importgenius.com/importers/k … eering-llc.

I've tried a number of times to get them to respond back via email as I am unable get in contact by them via phone, but have gotten no response.

Just to be fair, I have no problems with their PLA, works great, but avoid their ABS as it just doesn't work.

Just to be certain that it's not my printer (or me), can anyone spare a couple of meters of good working abs for me to try?

2

Re: Warning - BAD ABS supplier

Strange.. gotten two spools from them so far (white 1.75mm abs) and they print just as well as botfeeder/octave filament for me..  must have gotten lucky.