<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Warning - BAD ABS supplier]]></title>
		<link>https://www.soliforum.com/topic/5299/warning-bad-abs-supplier/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/5299/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Warning - BAD ABS supplier.]]></description>
		<lastBuildDate>Fri, 24 Jan 2014 20:13:42 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Warning - BAD ABS supplier]]></title>
			<link>https://www.soliforum.com/post/47636/#p47636</link>
			<description><![CDATA[<p>Strange.. gotten two spools from them so far (white 1.75mm abs) and they print just as well as botfeeder/octave filament for me..&nbsp; must have gotten lucky.</p>]]></description>
			<author><![CDATA[null@example.com (ITman496)]]></author>
			<pubDate>Fri, 24 Jan 2014 20:13:42 +0000</pubDate>
			<guid>https://www.soliforum.com/post/47636/#p47636</guid>
		</item>
		<item>
			<title><![CDATA[Warning - BAD ABS supplier]]></title>
			<link>https://www.soliforum.com/post/47630/#p47630</link>
			<description><![CDATA[<p>After having nothing but problems trying to print ABS with my SD2, I did a little research and discovered that KBELL Engineering (they sell ABS on Ebay) has had issues with their ABS, with a number of people having the same feeding problem that I have had.<br /><a href="http://feedback.ebay.com/ws/eBayISAPI.dll?ViewFeedback2&amp;userid=kbellenterprises&amp;myworld=true&amp;items=25&amp;iid=-1&amp;de=off&amp;which=negative&amp;interval=365">http://feedback.ebay.com/ws/eBayISAPI.d … terval=365</a></p><p>I also was able to determine that the ABS filament they sell apparently comes from China.<br /><a href="http://www.importgenius.com/importers/kbell-engineering-llc">http://www.importgenius.com/importers/k … eering-llc</a>.</p><p>I&#039;ve tried a number of times to get them to respond back via email as I am unable get in contact by them via phone, but have gotten no response.</p><p>Just to be fair, I have no problems with their PLA, works great, but avoid their ABS as it just doesn&#039;t work.</p><p>Just to be certain that it&#039;s not my printer (or me), can anyone spare a couple of meters of good working abs for me to try?</p>]]></description>