Topic: Extruding Filament (Stuck)

Hello,

I was changing filament colors, and instead of retracting the filament like you are supposed to do, i forgot and just snipped it, and then extruded thinking that the new color will push the old one down, but it didn't, so now it gets stuck, so the only thing i can do is retract the new color and cant extrude. Any help would be appreciated. Thanks

2

Re: Extruding Filament (Stuck)

Hello, I fixed it myself, if anyone else ever does this you need to to remove the "swing arm thumb screw" http://www.solidoodle.com/how-to-2/troubleshooting/

Thanks