I just got a surface pro 2 to use with my solidoodle 3 and I am having some weird issues compared to using the printer on my desktop windows machine. I copied all the settings as far as I can tell, but a couple of odd things. When I submit a print job the print goes to the center of the bed and basically touches the center of the bed and stays for like a 1-2 minutes before going back to start position and printing. All temps are up so it doesn't seem like its waiting for that. Then when the print finishes, after the bed is lowered the extruder moves to complete opposite end of start position and basically rams into the other corner of printer. It is basically smashing into it. So bizarre. I am using windows 8.1 pro and before was just using 8 I believe so wonder if that has anything to do with or is there something I am missing in settings. I had been using Mac OS X 10.9 but thought the only way to adjust my extuder feed rate was in in windows, maybe I'll try mac again.