Topic: Freezing up
We just got a new Solidoodle 2 printer yesterday. We were able to print a few things (not very well) last night. I am trying something else today and I can not get the printer to connect. It did one time but every time after it freezes. Every time I push the connect button the program freezes. I then have to restart the computer to be able to close the program. It is connected correctly and all lights on. I can click on everything else in the program (BEFORE hitting connect) and it all works correctly. AFTER I hit connect, nothing will work.
Also, I was reading that turning up the extruder temp will help with the plastic not bonding together. I did that but the temp just dropped back down. I hope I didn't mess anything up! The connection problem started after this.