Topic: Snapped Acrylic
Hello all,
The acrylic jigsaw has snapped on my Solidoodle and now I can no longer print. I have ordered a replacement from imakr but these guys can take weeks to turn around an order.
I had printed http://www.thingiverse.com/thing:111213 as a replacement but one of the parts didn't quite come out right.
Anyone willing to run one off and send me it so that I can do some Xmas prints ?
I'll reimburse for ABS and Postage.
Cheers!