Topic: I think I know the problem, but I want to get a second opinion.
So, I got my SD3 and I started printing again after a little hiatus since I lost my Macbook Pro. My new Mac Mini is powering my SD3 and she's holding up well if anyone is interested. Here is the problem. I have included pictures of the carabiner clip that I just printed. You may notice that the fill seems very stringy, and even the outside edges of the clip are very frail. It's not as solid as I was hoping for and I'm not sure what the problem with that was.
I did however do a little research and I just wanted to maybe get some back up on this. Do I need to set the flow rate and do an extruder calibration? I just wanna make sure before I go down the rabbit hole for something that isn't going to fix my problem. Thanks guys and have a great Sunday/Monday morning/afternoon/night!