Topic: Filament problem or more?
I'm a first time printer owner (the solidoodle 3) and I've had the thing less then a month. Been largely smooth printing, but I have no clue what I did wrong here. Not certain if I should be blaming the filament or the extruder. I'm attempting to avoid removing the extruder, but if I have to I will.
It was printing great yesterday, and as you can see the more finished print was done first, it started failing in the middle of the print. All attempts afterwards fail in the first ten layers. I've tried removing and putting the filament back in. It extrudes great but than does this when printing. I'm not sure what other sort of things I should be trying to check first before I attempt to take the thing apart.