1

Topic: .1mm prints won't stick but .3mm will.

It's a very strange problem: .1mm prints won't stick but .3mm will. And the .3mm prints stick VERY strongly. I've tried using a brim.

On the rare occasion that they do stick the print's edges curl up around the nozzle. They don't peel off from the bed though, the extruded plastic just curls upward.

Using a glass bed with hairspray at 100c.  205c extrusion temperature.


Also: Slicer is ignoring temperature settings and is just defaulting to 200c, even if I change the default temperature. So I'm having to pause prints right at the start to set the temperature higher.

2

Re: .1mm prints won't stick but .3mm will.

Yap that is because the bed is calibrated for 0.3 you need to calibrate it for 0.1.

at least for me each time I pass through  one or the other I have to level the bed accordingly.

3

Re: .1mm prints won't stick but .3mm will.

Yep. You think it wouldn't matter since the first layer is supposed to be .3mm in both cases. =o\

Still having problems with the temperature settings in filaments not being obeyed.