I have been calibrating my Solidoodle 2 so far Im happy with my results with PLA, but can someone guide me on how to fix the top layer the bridging and infill looks off, attached are some pics.

Post's attachments

20130915_131103.jpg
20130915_131103.jpg 1.37 mb, 1 downloads since 2013-09-15 

20130915_131200.jpg
20130915_131200.jpg 1.66 mb, file has never been downloaded. 

20130915_131235.jpg 1.69 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2 (edited by 3d-oodler 2013-09-15 22:10:00)

Re: PLA Calibration Help

What temp are you printing at?

It looks too hot to me.

I was printing PLA @ 150C with the stock hotend, but generally aimed to print close to the lowest temp that I could where the material was easily pliable...as measured by extruding to the side of the bed and seeing how it folded over an object or wound in a circle on the floor of the printer.

3

Re: PLA Calibration Help

Im printing at 185 I cant print under 170 with out doing firmware change

4

Re: PLA Calibration Help

Use gcode M302 to allow for cold extrusion and test colder temps.

You send m302 once and it lasts the whole session.

5

Re: PLA Calibration Help

Thanks for the advice I changed the values in my firmware instead the PLA material that I have melts best at 170 c any lower and it will jam