Topic: SD3 exttruder motor not turnning
I got my printer in April. While trying to print I used up the filament that came with the printer and maybe a meter of white from Amazon. While we were backing out the filament the motor just stopped. Some details are a bit fuzzy, but working with support we decided that the motor was bad. (yes I know how unlikely ) After my screwup with Paypal (wrong email 30 days) the new motor arrived. No change! We double check all the driver chips for the right voltage. Next SD sent a new driver chip for the extruder, no change. So here is a list.
Changed motor
Changed driver
Swapped mother board
Installed latest mother board(SD)
Frustrating of course. Just to fit things together. I am a 78 year old retired mechanical engineer with MS. The motivation to get the SD was that I saw a way to make parts on my desktop. I had been interested in rapid prototyping since about 93. Then I ran across the idea of desktop DIY printers and began designing one. So here I am asking for help.
Thanks for reading this story.
Lowell