Topic: ABS warping and bed temperature
This from the Trinity Labs A1 forum:
Sep 11
Here is my first big ABS part. No curling or warping in the corners! I'm printing at 233C at the head and 105C for the bed. The TG point of ABS is approximately 100C. To relieve the internal stresses in the part, the bed temperature must therefor be higher than the TG. As soon as I realized that (I had been printing at 95C), no more problems.
https://groups.google.com/forum/#!topic … kz_BaA2fFg
If this turns out to be true, there may be a fundamental design flaw in the newer Solidoodles (where the bed temperature is limited to 80C, if my memory is correct).