Topic: The Dark Knight
Thigiverse 90594
SD2 at .1mm
20secs acetone vapor bath(Presto Kettle)
Rustoleum Oil Rubbed Bronze.
He's sitting under a bright light so the metallic effect of the paint is more pronounced,in the display case it gives the appearance of an oiled bronze sculpture.
I feel detail is harder for the eye to pick out if the print is left a high gloss so I've gone to satin finish Rustoleum paints to do my .1mm prints.The detail of his face mask and chest emblem were hard to make out in gloss abs but "popped" when painted.
There are a few very minor ridges if you take a hard look but I wasn't about to chance a 2nd exposure to the vapor and make a good looking print go "fubar".