Like the title says im not having any problems with my printing (aside from the large print warp age but im addressing that right now). But what settings are you guys using to print ABS as far as temps?
Im running my extruder at 203 and my bed at 118 which from what im reading is pretty hot. But i havnt had any problems with it and it seems to lay down better and bond better. Just curious really nothing else.