1

Topic: No problems...just curious

Like the title says im not having any problems with my printing (aside from the large print warp age but im addressing that right now).  But what settings are you guys using to print ABS as far as temps?
Im running my extruder at 203 and my bed at 118 which from what im reading is pretty hot.  But i havnt had any problems with it and it seems to lay down better and bond better.  Just curious really nothing else.

Thanks
Chad

2

Re: No problems...just curious

Chad,
These temperatures should be fine

Former Solidoodle employee, no longer associated with the company.

3

Re: No problems...just curious

That's about what I'm running mine at. Seems to be working well.

SD3 w/ RUMBA (8825s), merlin hot end (in pieces). Ender3 w/ silent board for PLA printing. Ender5 w/ silent board, e3d v6, new z lead screw, and glass bed. DiY Kossel w/ smoothieboard (in pieces). Vellman Vertex (in pieces)
Shapeoko2 router in process of being converted to laser engraver (in pieces)
Multicam 5000 series CNC Router w/ 11HP spindle, 5x10' table, and auto tool changer (in pieces)