dubbsd wrote:The thermistor came unplugged during print from what I can tell
it had been unplugged about 7 minutes.
the peek melted enough you can not see the barrel between the peek and block.
so I now have to set up the ceramic peek hotend that I have had a few weeks.
this doesn't sound like it was the thermistor that came unplugged. The Marlin firmware has a saftey built in that shuts everything down if the thermistor stops reading. You might want to check to see if the gate on the mosfet is stuck open. Measure the voltage of the extruder port without "heat extruder" turned on. If you have 12V then the mosfet is stuck and you should get a new one.
SD3 w/ mods:
Glass bed with QU-BD heat pad upgrade, threadless ballscrew w/ 8mm smooth rod, spectra line belt replacement, lawsy MK5 extruder, Lawsy replacement carriage, E3D hotend, Ramps 1.4 w/ reprap discount controller, DRV8825 drivers, 12v 30A PS, Acrylic case, Overkill Y-idlers, Filament alarm, Extruder fan + more.