2n2r5 wrote:you might need to check your retraction settings. Trying turning the retraction length down(extruder settings) for this filament. Also, what temp did you extrude at? It looks like you had some issues with the layers not sticking together well. Maybe try to bump it up 5 degrees or so.
It looks like you are going the get an amazing print when you get this cleared up.
If I remember correctly this was printed at 200c with 100c bed, if not it was 195/95. I get these 'blobs' occasionally with other prints at .3mm, but it occurred much more frequently with this print. I've done a fair amount of printing since I got the printer a little over a month ago, haven't had any issues with layers sticking. This may be an anomaly since the vase walls are so thin and called for 0 infill. My main concern is figuring out what causes those blobs of ABS.
I've done a lot of the calibrations, but haven't looked into retraction settings. Will check it out, thanks!
E3D-v4 Hotend, MK5 carriage with round plastic wire conduit , 3/16" tempered glass, Well nut, SureStepr SD8825 1/32 Extruder Driver, PowerEdge 2650 500W PS, QU-BD heated bed, circuit board fan, hinged plexiglass enclosure with plastic tray top. Other than that mostly stock SD3