1

Topic: Temperature settings issue

Hi everyone, I have a big issue with my temperature setting.

It just won't measure the reality. When my extruder and bed reach a high temperature, repetier see a lower one. How can I solve this ?

I join a picture, obviously my extruder was at much more that 70C after 2 min of heat and so for my bed.

I bought my solidoodle 3 5 month ago and i still couldn't print anything. I'm desperate could you help me ?

2

Re: Temperature settings issue

What temperatures are being displayed, please give us an example.. is there a 30 degree difference or is it a larger difference? is the problem for both the extruder and the bed heater? some screen shots would be a great help to know what is happening with your SD3.

No picture in your above post.

3

Re: Temperature settings issue

Hi Ronsii

Thanks for your interrest

Actually, there are no temperature related to the reality, When I Heat the bed and / or the extruder the temperature rise but with a few degree where in reality it's really hot.

The actual temperature is 70C for the extruder witch is wrong and 7C whitch is also wrong.

Here a re some pictures.

I also try to upgrade the firmware and nothing work too ... it's fucking depressive

Post's attachments

SD3 Problem 2.png
SD3 Problem 2.png 183.18 kb, file has never been downloaded. 

SD3 Problem.png
SD3 Problem.png 159.78 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

4

Re: Temperature settings issue

Either you found a bug in repetier... .85 has some small bug fixes compared to .82b... or the thermistor type is set wrong for the hotend.

one other possibility is a hardware problem or wiring problem with the thermistor.