looked good till it got 30mm off the bed. i don't have a case. i feel this may be a big part of the problem. either that or my x stepper fan blows on the bed once it gets to that height. printed at .3 layer height.

Post's attachments

2013-05-12_18-30-34_666.jpg
2013-05-12_18-30-34_666.jpg 1.27 mb, file has never been downloaded. 

2013-05-12_19-51-49_400.jpg
2013-05-12_19-51-49_400.jpg 1.29 mb, file has never been downloaded. 

2013-05-12_22-11-55_100.jpg
2013-05-12_22-11-55_100.jpg 948.03 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: Looks like thermal banding?

In the third photo, the banding is caused by the small area of those layers either side of the hole. The plastic doesn't have time to cool properly so distorts. Using a fan will assist here.