CrazyBear wrote:Is it safe to set the extruder to 205C or more? I got a reply from Octave support and they recommended to set up the temp higher.
In fuller detail for anyone else ever reading; Solidoodle reported temps are about 30°C *below* the highest temp in your heater core. So this is why people use 190°C to print ABS that normally requires 220°C.
The item that suffers the most in high temps is the PEEK holder section - It has a failure tempreature of 250°C. Knocking 10°C off this for 'safety' and to deal with overshoot, you can run the Solidoodle at temps up to 210°C without problems, but I would not exceed this temp as you then are well approaching the PEEK failure temp.
Nutshell version - 205°C is ok, but I wouldn't push past this. And thats already 235°C 'actual', so I wouldn't expect the filament to need more than this anyway if its within standard parameters.