Topic: Fill patterns and when to use them
I know what the general difference between rectilinear and concentric are. (Rectilinear is basically a square pattern, whereas concentric follows the profile kinda like the rings in a tree trunk).
When should each be used for best print quality/speed? I'm guessing rectilinear for primarily square object and concentric for round or more organic objects. But what about a mixture of the 2? i.e. a square profile with holes, round extrusions, fillets and ribs?