1

Topic: At wits end

Here are some parts that I printed when I first got my SD 3 ,as you can see  they look pretty good. Edges are smooth and and have well defined features.But now after the hotend that failed ( after only 2 weeks) and was replaced, I can't as hard  as I try to duplicate those parts.I did replace the jigsaw with the MK4 and new hotend ( a couple of HE actually) I have also tried several versions of RH and slic3r. I have done bed leveling ect  and all that per here on the forum and the wiki's. I just run out of ideas. All I am doing now is wasting filament.

Post's attachments

PARTS.JPG
PARTS.JPG 93.46 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.
SD3, E3D hotend,linear bearing on x/y axis',pillow block bearing on y conneting rod, ball bearngs on front y axis, fan on y stepper motor.

2

Re: At wits end

What do they look like now?