1 (edited by Mistr_K 2013-04-13 20:06:36)

Topic: Hot End temps change randomly [Fixed]

For some reason, my hot end temperature keeps changing from what I set it as. I've tried searching for a solution online, but the only thing I come up with is changing the PIDs (which I've done 3 times). Does anyone know what would be causing this?

I have one of the newer hot-ends if that makes a difference.

Thank you!

2

Re: Hot End temps change randomly [Fixed]

The setpoint is changing, or the actual value?

3

Re: Hot End temps change randomly [Fixed]

How many times does it change from when you start a print until it finishes?

4

Re: Hot End temps change randomly [Fixed]

I'm an idiot. I didn't check my gcode, it's changing the hot-end temperature every time I print.

Thanks!

5

Re: Hot End temps change randomly [Fixed]

Hey, no prob... just glad it was something simple smile