Topic: Recomended ABS

Hi everyone,

Mabee a stupid question, but why is ABS recommended vs. PLA?

I would like to use mainly PLA in my soon to order Solidoodle 2 expert...

Thanks for your responses :° )

www.designerfred.fr      before: Solidoodle 2 + E3D v6 now: MeCreator II and OLO 3D

2

Re: Recomended ABS

For me the main advantage is being able to use acetone to smooth the part. Search for this if you haven't seen it before.

3

Re: Recomended ABS

Thanks Lawsy, Yes I've seen the posts about that... I'm going to keep to PLA for indoor "appartment" printing, to keep the fumes healthy, hopefully at high res., like 0.1 or 0.15 layers.

www.designerfred.fr      before: Solidoodle 2 + E3D v6 now: MeCreator II and OLO 3D

4

Re: Recomended ABS

I asked the same question in IRC and the Solidoodle tech said it was mostly that it's because that's what the Solidoodle staff are most familiar with.

I have a spool of PLA to give a try with, though I don't think it's likely to offer a different result with my stair-step problem.

5

Re: Recomended ABS

Hunter, Being a machinist cnc in another life, looks like belt skipping to me! Measure one tooth, and one space on the Y belt, I bet its the same space on your step. Belt may be too tight, or too loose!

www.designerfred.fr      before: Solidoodle 2 + E3D v6 now: MeCreator II and OLO 3D

6

Re: Recomended ABS

Oh, and thanks for your reply to my question... :0)

www.designerfred.fr      before: Solidoodle 2 + E3D v6 now: MeCreator II and OLO 3D

7 (edited by Leghk 2013-04-07 17:20:18)

Re: Recomended ABS

DesignerFred wrote:

Hi everyone,

Mabee a stupid question, but why is ABS recommended vs. PLA?

I would like to use mainly PLA in my soon to order Solidoodle 2 expert...

Thanks for your responses :° )

The key differences for me are:

  • ABS prints have a little flexibility, PLA is very stiff

  • PLA shrinks less than ABS, less warping during prints

  • ABS can handle higher temperatures before it softens

  • and some PLA smells like waffles while printing smile

Don: Folger Tech 2020 Kossel Rev A + Borosilicate + Snow Effector
        Davinci 1.0 + Repetier : Filastruder
        SD3 + RAMPS + Lawsy Carriages + E3D + Borosilicate + ... : Cupcake

8

Re: Recomended ABS

Thanks, I like Waffles smile

www.designerfred.fr      before: Solidoodle 2 + E3D v6 now: MeCreator II and OLO 3D

9

Re: Recomended ABS

Waffles? That's terrific. smile I think scratch and sniff 3D modeling is the way of the future. lol.