1 (edited by Kvirre 2013-03-21 10:55:14)

Topic: Move / Retract-filament between objects

When my extruder jumps / moves between objects it leaves strands of plastic since it does not seem to retract efficiently? Or is this a problem with speed or heat?

What do you suggest to try?

Post's attachments

image.jpg
image.jpg 1.3 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: Move / Retract-filament between objects

Have you tried increasing the retraction amount?

3

Re: Move / Retract-filament between objects

No, not yet since this is the default settings, and I see this as a "last resort"

What's different now from then, is the following :

Extruder Calibration is done
Jigsaw replacement added
gcode fan-controll added

4

Re: Move / Retract-filament between objects

Ok, I solved the problem by adding additional retract from 1 mm to 2 mm.
Strange that I did need to to that though.

5

Re: Move / Retract-filament between objects

It's normal, and sometimes changes between spools and colors, don't worry about it.