Topic: Da Vinci Jr: Extruder Cooler?
My extruder is heating up and flattening filament on complex prints with lots of retracts. Has anyone made a mod to work around this? I'm wondering if I can remove the casing to let it breathe more, or add a fan but haven't found any evidence that this has been tried.
No, I'm not talking about a fan for the hotend but rather for the extruder ![]()