Topic: XYZ Mini Maker clogs at exact same spot (%32)
Hey, there. I have this machine for a long time. I usually use this for short prints because it clogs for no reason at long prints( I use Ender 3 for this). The problem is the machine just clogs at the same spot or for no reason. It says "filament jam" even though filament is extruding and no jam. I used default filament that comes with the printer itself and the same result. And with my own PLA, it is the same. Gears are clear as I clear them regularly. The nozzle and extruder are clean (as I clean regularly).