Topic: Auger not going inside the barrel
Hello,
I ordered 2 Filastruder kits and received my package yesterday. When checking everything, I tried to insert the Auger in to the Barrel. In one barrel, auger is not going all the way inside, it only goes 1-2 cm. In other kit, Auger goes inside but it doesn't stick out the barrel at all. Assembly manual says,
If more than 10 mm or less than 2 mm of the feed screw sticks out, contact support.
What should I do?
Tried interchanging augers, same result.
Hope the attached picture helps.
Thanks