Topic: need to remove glass from build plate that has hairspray holding it
what cuts hairspray or can I heat bed to get glass loose without breaking it?
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → 3D Printer Discussion → need to remove glass from build plate that has hairspray holding it
what cuts hairspray or can I heat bed to get glass loose without breaking it?
what cuts hairspray or can I heat bed to get glass loose without breaking it?
Just take a paint scrapper and slid it between the glass and plate slowly. The glass will come loose.
yup, what carl said.. use a putty knife/scraper, slide in between glass & bed, and work around the perimeter with it.. it should pop loose once you get far enough around.
SoliForum - 3D Printing Community → 3D Printer Discussion → need to remove glass from build plate that has hairspray holding it