Topic: Print quality is great on one object but crappy on another
Ok, this has never happened to me before. I use my jr1.0 alot. Whenever i print i 95% of the time use the following:
Good quality
standard speed
10% infill
normal shells
0.3 layer height
no increase in temp
4mm retract length
30 retract speed
XYZ PLA CLEAR BLUE
My print have always come out amazing with these settings. I am using the clear blue. then today, i made something on the same settings and it came out crazy looking. lots of theese little snake looking pieces hanging from it. I am wondering if it has something to do with the shape of the object. Here are some pics, first showing the great quality, then the not so great






Im wondering if it has something to do with the thin walled circles. they are 1.25mm thick, i did try with 2mm thick walls and it was terrible, but in the first or second photo, with the clear green, you can see how it handles the thin walled rim just fine.
thanks for looking:)