Topic: Extruder temp running low
I took my meter and checked the nozzle temp. and it is running low.
I set the printer to warmup to 230°c and it heats the Nozzle tip to 197°c
I am thinking this is a lot of my printer problems and need to raise my temp 33°c
that is 33°c lower than recommended for ABS.
I use hatchbox ABS.
could the problem be a hardware problem?
My meter is a Calibrated meter.
Thanks