Topic: Help - XYZ Da Vinci 1.0 JNR
So had this printed 2 days now and each time the plastic tube comes out of left extruder and doesnt push into the printer head. Any ideas why ?
Thanks
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → 3D Printer Discussion → Help - XYZ Da Vinci 1.0 JNR
So had this printed 2 days now and each time the plastic tube comes out of left extruder and doesnt push into the printer head. Any ideas why ?
Thanks
elcheapo bowden tube connectors . buy some good connectors and some good tubing
Any recommendations as to where to get them and which
thanks
https://www.printedsolid.com/collection … n-coupling
https://www.printedsolid.com/collection … 7610453836
the top two are premium parts
https://www.printedsolid.com/products/ptfe-tubing
https://www.folgertech.com/products/2me … ap-rostock
https://www.ebay.com/itm/Push-Fit-Pneum … itleDesc=0
I've been using my Jr 1.0 with no problems with the feed tube. There is only 1 extruder and it's on the right side of the printer if you are looking at it. The feed tube connects to the filament feed drive on the left and you need to insert the tube about 3/4 of inch into the tube fitting. It's easier if you ease the left side open to help guide the tube in. Push it in, until it seats. This is the same type of tube fitting that's on the extruder, with the little black spring release ring on top.