Topic: [Da Vinci 2.0a Duo] ABS not sticking [Slic3r]
I leveled my bed to many times.
Used auto level bed and touched everything else.
But Or it will not stick using a glue-stick and a heated bed.
Or it clogs up a round the nozzle when i use 4 stick layers of glue.
I'm now playing with the z-offset setting in slic3r itself.
below my settings, if someone could help me figure out where i'm going wrong.
I would love the help ![]()
I bet is scewed up my PLA settings also ![]()
Manual bed leveling:
paper 0.12 mm thick
Zmin evaluation:
Z1 = -4.744 mm
Z2 = Failed
Z3 = ......... mm
manual set Zmin to zero
ABS diameter 1.75 mm
flow/multiplier 0.9
extruder 230c first layer and others
bed 95c first layer and other
first layer 0.3 mm
other layers 0.2 mm