Topic: Filament Diameter
What diameter do most of you use when extruding 1.75 filament? I have noticed if I extrude right at 1.75 or a couple thousands smaller I get a lot of nozzle jams and my prints fail. I backed down the diameter to 1.62 and changed my slicer settings and it seems to work without jams. Just wondered if others have this same issue and how it was corrected.
Thanks