dubbsd wrote:what is the secret to not having bubbles in the tape. I have tried starting it and using a squeegee to lay it down
and end up with bubbled. I have used Windex so it wont stick (like applying decals) and when I heat the bed I have bubbles.
I have fought this for years.
I am running a stock Makerbot and do not want to change to glass and hairspray or gluestick.
Thanks
Dale.
I don't use tape, I use glass + glue stick, works great. I do read somewhere mention use soapy water to lay out kapton tape.
Windex is not soapy water, it contain ammonia which generate bubble after almost dry.
Make soapy water from the actual soap or handwashing/dishwashing liquid.
http://forums.reprap.org/read.php?1,124034
https://www.makerbot.com/media-center/2 … ut-bubbles
https://en.wikipedia.org/wiki/Windex
(Da Vinci 1.0, Jr. 1.0 RAMPS, miniMaker) X4, (Creality CR-10S, CR-10 mini, Ender-3) X4, Anycubic MEGA X4, Anycubic Chrion X1, ADMILAB Gantry X2 (MonoPrice Maker Select V2, Plus, Ultimate)X4--Select mini X1, Anycubic photon X4, Wanhao duplicate D7 X1.