Topic: room temp vs bed temp
If the ambient room temp is about 68 say , that being a bit cool. Should the bed temp be set higher than normal? ( I have it at 101 now)
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Solidoodle Discussion → room temp vs bed temp
If the ambient room temp is about 68 say , that being a bit cool. Should the bed temp be set higher than normal? ( I have it at 101 now)
Not necessary, but you should consider enclosing your build environment, even if it's plexiglass and magnets or even cardboard would work. Warping and peeling all but vanish after doing this.