1

Topic: Filastruder : Heater issue

Hi here !

I'm the 3043 Filastruder smile

I mounted it today, and wired it like in the manual, just without the 2 switches because they are not in the box sad

2 fans are okay, feed screw turn well, temperature sensor working perfectly, but the heater doesn't heat.

I'm not sure to do the write thing to start the heating.

My Filastruder came with a Stestos d1s-2r.

If you have any idea.

Je suis Français, mais je ne mord pas wink

2

Re: Filastruder : Heater issue

you need those switches. the machine needs to get to a stable operating temp before you start trying to extrude. You should write Tim an email. As for the heater Id check the wiring after you add the switches

Sd4 #9080 with a glass bed. E3d chimera duel extruder. Paste extruder , duet wifi.
Lawsy carriages. linear bearings. Y axis direct drive, Kinect scanner
SD4#8188 glass bed, lawsly carriages, E3d v6, octoprint http://www.ustream.tv/channel/hotrod96z28
Filastruder/filawinder, Custom Delta 300mm x 600mm

3

Re: Filastruder : Heater issue

Thank you Kronikabuse, I have write a mail about that already, but its not really the point of this topic, I don't want to extrude without heating at correct temperature. Except switches, wiring is almost the same than the manual : heater is on pin 7 and 10 of the PID, and except heater, every other pieces working well.

But maybe I don't know how to start the heating process on the PID, set the correct value and run ?

Perhaps my heater is defective.

Pour les Français, je suis Français wink

Je suis Français, mais je ne mord pas wink

4

Re: Filastruder : Heater issue

I haven't received any email about missing switches.

Do you have a jumper between pin 8 and pin 9 as described in the instructions?
What is the resistance of the heater when not connected to anything else?

5 (edited by arthak 2017-09-12 09:15:06)

Re: Filastruder : Heater issue

Wow. Kill me.

This is really a nooby thing, I forgot to strip the insulation of wires.....

This working well now !!!

Elmoret, I've write it but not sended wink Is in your mailbox now smile

Thank you !

Je suis Français, mais je ne mord pas wink