Topic: Extrusion problems

So my Davinci Jr. is only printing on half of the table. I followed the cleaning instructions and cleared a blockage yet it still only prints on the side closest to the filament spool. on the far half of the table it only leaves a heat impression on the table but no filament. and the driver clicks repeatedly how do I fix this?

Post's attachments

19961393_1873246466035430_1071865390618470947_n.jpg
19961393_1873246466035430_1071865390618470947_n.jpg 37.43 kb, file has never been downloaded. 

19990356_1873246442702099_1139416050324753047_n.jpg 29.94 kb, file has never been downloaded. 

20032056_1873246412702102_7455383678158284605_n.jpg
20032056_1873246412702102_7455383678158284605_n.jpg 37.47 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: Extrusion problems

sounds like you need to level the table.

Soliddoodle 4 stock w glass bed------Folger Tech Prusa 2020 upgraded to and titan /aero extruder mirror bed
FT5 with titan/ E3D Aero------MP mini select w glass bed
MP Utimate maker pro-W bondtech extruder
Marlin/Repetier Host/ Slic3r and Cura

3 (edited by Bozotclown1970 2017-07-15 17:12:47)

Re: Extrusion problems

Kitt_Beesley wrote:

So my Davinci Jr. is only printing on half of the table. I followed the cleaning instructions and cleared a blockage yet it still only prints on the side closest to the filament spool. on the far half of the table it only leaves a heat impression on the table but no filament. and the driver clicks repeatedly how do I fix this?


Tin Falcon was 100%. Here is how I took care of that problem on my JR. There should already be a threaded hole o n the right side of the extruder support bar. I believe it is 4 or 5mm, check to make sure. Use the paper trick to adjust the Z axis. See attached for complete fix.


http://soliforum.com/i/?dfJxBMF.jpg

4

Re: Extrusion problems

thanks guys this seems to have fixed the issue

5

Re: Extrusion problems

Mr Clown, that is a great solution.  Do you find that the adjustment bolt loosens over time form the vibration?  The single wing nut hold it well?

6

Re: Extrusion problems

mjf55 wrote:

Mr Clown, that is a great solution.  Do you find that the adjustment bolt loosens over time form the vibration?  The single wing nut hold it well?



The wing nut seems to hold it just fine.