Topic: Broke the thermistor, where to buy a new one?
So long story short, I was cleaning out a jam which caused a huge ball of melted filament to form inside the extruder assembly. After I was finished cleaning it out I tried to print again and noticed that the temperature just sits at 10 degrees. I guess while I was cleaning out the extruder I somehow snapped something inside of the thermistor. I know it is the thermistor and not the heater because the extruder heats up enough where i can extrude filament by pushing it through by hand, but the display reads out 10 degrees. I was wondering if/where I can buy a new thermistor for my Da Vinci JR 1.0 because I really do not feel like paying $80 for an entire new extruder as XYZ Printing customer service is telling me (printer is out of warranty) when only a tiny part of it is broken.