Topic: No pillars on my overhangs!
Hi guys, my 1st post here.. having a nightmare with the slic3r settings on my solidoodle press....
I'm using soliprint and trying to print something that has a 45 degree angle (see pic below), but nothing I do will get the support pillars to generate!(slic3r settings are also below.)
Does anyone have a clue for me? Many thanks in advance ![]()