Topic: Help: Weird Lines/Wobble along print
Hello all,
I just did my first large print and it has some inconsistent lines along the surfaces.
The lines are only on the 2 sides of the print, and it was printed diagonally on the print bed due to the size.
And idea what is causing this issue?
Printer is an Anet A8.
Thanks!